Mobilgear 600 XP | 68 | 100 | 150 | 220 | 320 | 460 | 680 | ISO 粘度等级 | 68 | 100 | 150 | 220 | 320 | 460 | 680 | 粘度,ASTM D 445 | | | | | | | | mm²/s @ 40 ºC | 68 | 100 | 150 | 220 | 320 | 460 | 680 | mm²/s @ 100 ºC | 8.8 | 11.2 | 14.7 | 19.0 | 24.1 | 30.6 | 39.2 | 粘度指数, ASTM D2270 | 101 | 97 | 97 | 97 | 97 | 96 | 90 | 倾点, °C, ASTM D97 | -27 | -24 | -24 | -24 | -24 | -15 | -9 | 闪点, °C, ASTM D92 | 230 | 230 | 230 | 240 | 240 | 240 | 285 | 密度,@15.6 ºC, ASTM D4052, kg/l | 0.88 | 0.88 | 0.89 | 0.89 | 0.90 | 0.90 | 0.91 | FZG微点蚀,FVA 54,失效阶段/额定 | | 10 / 高 | 10 / 高 | 10 / 高 | 10 / 高 | 10 / 高 | 10 / 高 | FE 8 磨损试验, DIN 51819-3, D7,5/80-80. 滚柱磨损, mg | 2 | 2 | 2 | 2 | 2 | 2 | 2 | 铁姆肯OK负荷, ASTM D 2782,磅 | 65 | 65 | 65 | 65 | 65 | 65 | 65 | 4 球 EP 试验, ASTM D2783, | | | | | | | | 焊接负荷,kg | 200 | 200 | 250 | 250 | 250 | 250 | 250 | 负荷磨损指数,kgf | 47 | 47 | 47 | 48 | 48 | 48 | 48 | FZG划擦,DIN 51354,失效阶段 | | | | | | | | A/8.3/90 | 12+ | 12+ | 12+ | 12+ | 12+ | 12+ | 12+ | A/16.6/90 | | 12+ | 12+ | 12+ | 12+ | 12+ | 12+ | 防锈保护, ASTM D665,海水 | 通过 | 通过 | 通过 | 通过 | 通过 | 通过 | 通过 | 铜片腐蚀,ASTM D130, 3 小时 @ 100 ºC | 1B | 1B | 1B | 1B | 1B | 1B | 1B | 抗乳化稳定性能,ASTM D1401,3ml乳化时间,分钟@ 82ºC | 30 | 30 | 30 | 30 | 30 | 30 | 30 | 泡沫试验,ASTM D892,趋势/稳定性, ml/ml | | | | | | | | 顺序1 | 0/0 | 0/0 | 0/0 | 0/0 | 0/0 | 0/0 | 0/0 | 顺序2 | 30/0 | 30/0 | 30/0 | 30/0 | 30/0 | 30/0 | 30/0 | |